A shipment of mullite bricks can look perfectly sound on arrival and still be a poor choice for a loaded pusher plate. Creep is gradual deformation under sustained heat and load, so I would not try to judge resistance by appearance alone. My receiving check would answer two separate questions: did the supplier deliver the specified grade, and is there evidence that this batch will resist deformation under the conditions where we plan to use it?
I would start with the purchase specification and the supplier’s batch paperwork. A claim such as “low creep” is not enough on its own. I would ask for the reported creep result and the conditions behind it, including the applied load, temperature, and time. Without those conditions, I cannot tell whether the result is relevant to a loaded pusher plate. I would also make sure the paperwork identifies the delivered batch rather than merely describing the product grade in general.
Next comes sampling the bricks that actually arrived. For load-bearing areas of a high-temperature pusher kiln, the supplied guidance recommends a bulk density of at least 2.60 g/cm³. I would check density on the incoming samples because a lower-density product being supplied as a high-density grade is a real concern. But I would not treat a passing density check as proof of creep resistance. Density helps verify what was delivered; a creep test addresses how the material deforms under sustained high-temperature load.
For a critical load-bearing position, I would have representative incoming samples tested for creep and compare the result with the agreed acceptance requirement. The test conditions matter as much as the final figure: a result measured under conditions unlike the intended service conditions can be reassuring without being useful. If the purchase documents never defined an acceptable creep result or test conditions, I would resolve that gap before accepting the shipment for the critical location rather than inventing a pass mark after the fact.
I would also inspect the bricks for damage and confirm that their dimensions suit the installation. That does not verify creep, but it can prevent a separate problem: extensive cutting of pusher plates creates cut surfaces that may become starting points for stress cracks. Finally, I would keep the service plan in view. The supplied guidance advises against long-term use above 1600°C because deformation can accelerate. A sound arrival check cannot compensate for operating the brick beyond the conditions it was selected to handle.